ExtragentAnalytical chemistry of precious metals
Extragent DOS in a flask

Product

Extragent DOS (di-n-octyl sulfide 98.8%+)

Analytical extractant for the determination of gold, platinum, iridium and other precious metals in natural and technogenic materials

≥ 98.8 %DOS content
≥ 3.22mol/L
0.844density, g/cm³
258molecular weight
5 yearsshelf life
1 Lpackaging

Specification

AppearancePale yellow liquid
Molar concentration, mol/L, min.3.22
DOS content, % by weight, min.98.8
Density, g/cm³0.844
Molecular weight258
Sulfide sulfur content, %12.3
CAS No.2690-08-6

Typical use for gold assay

Gold is extracted from an acidic chloride solution (after aqua regia digestion) with a solution of DOS, most often in toluene; the concentration is set by your laboratory's method. The ideal diluent is aviation kerosene (grade RT): the kerosene extract allows maximum aspiration in the flame and can be introduced into ICP-OES, whereas a toluene extract requires reduced aspiration in an air–acetylene flame and special introduction devices for ICP. Measurement: flame AAS (Au 242.8 nm) or ICP-OES (Au 242.795 nm, 267.595 nm).

Detection limit, Aufrom 0.003 g/t (ICP-OES); from 0.05 g/t (flame AAS)
Consumptiondepends on your method; indicatively 1 L ≈ 6,500–8,000 determinations
Selectivitypractically only palladium is co-extracted with gold; iron does not interfere

Working parameters follow your laboratory's validated method. We can send the texts of the standard methods (GOST, NSAM; in Russian) on request.

Packaging, storage, delivery

  • Packaging: 1 L bottles. Price on request.
  • Storage: in a dark place at not more than 40 °C; shelf life not less than 5 years.
  • Documents: certificate of analysis for each batch, safety data sheet.
  • Delivery within Russia: 10–15 days; international delivery by agreement.